150x50
 

Specific Applications Film

UHBM

ULTRA HIGH BARRIER ONE SIDE METALISED OTHER SIDE HEAT SEALABLE FILM

 
tds

VACUUM DEPOSITED ALUMINIUM LAYER

METALLISABLE, HIGH SURFACE ENERGY LAYER

INTER LAYER

OPP CORE LAYER

INTER LAYER

TREATED/UNTREATED HEAT SEALABLE LAYER

t6s
Description

 ULTRA HIGH BARRIER ONE SIDE METALISED OTHER SIDE HEAT SEALABLE, ONE OR BOTH SIDE CORONA TREATED FILM

Features
  • Outstanding Oxygen Barrier
  • Outstanding Moisture & Light Barrier
  • Good Treatment retention & metal adhesion
  • Extended shelf life for food products
  • Replacement of Al foil
  • Easy processing at high Speed
Application

  • Pouch/Sachet Laminates
  • Health and beauty care
  • Dry foods and beverage powders
  • Biscuits, cookies & crackers packaging 

THE BIG DIFFERENTIATORS

01

ULTRA HIGH BARRIER

Extended shelf life for food products by 50% retaining classical freshness, crispness & aroma.

02

Replacement of Aluminum Foil

Outstanding Oxygen, Moisture & Light barrier

03

Excellent Metal Bond

Durability & sustainability of barrier under extreme conditions. much stronger extrusion/adhesive bond strengths.

04

Good Resistance to mineral Oil

Absolute protection of oxidation for cattle chips with significant fat content.

05

Chlorine free solution

Environment friendly & non-carcinogenic

PROPERTIES TEST METHOD (ASTM) UNIT TYPICAL VALUES
UHBM-15 UHBM-18 UHBM-20
PHYSICAL
Thickness ASTM D 374 MICRON
15 18 20
Grammage NTM gm/m²
13.65 16.40 18.20
Yield NTM m²/kg
73.3 61.0 55.0
Thickness variation %(±)
SURFACE
Treatment Level (min) ASTM D 2578 dyne/cm 38
OPTICAL
OPTICAL DENSITY
NTM

-

2.70

MECHANICAL
Coefficient Of Friction ASTM D 1894

Static

Kinetic

0.40-0.45

0.35-0.40

Tensile Strength

MD

TD

ASTM D 882

kg/cm²

1200-1500

2600-3000

Modulus

MD

TD

ASTM D 882

kg/cm²

16000-18000

26000-28000

Elongation

MD

TD

ASTM D 882

%

140-160

40-80

THERMAL
Shrinkage at 120°C/5min

MD

TD

ASTM D 1204

%

2.0-4.0

1.0-3.0

Seal Initiation Temperature (Max)

NTM

°C

105-115

Sealing Strength (min) at 120ºC/2Bar

NTM

gms/25mm

300-400

BARRIER
Water Vapour Transmission Rate ASTM F 1249 gm/m²/24h
≤ 0.10 ≤ 0.10 ≤ 0.10
Oxygen Gas Transmission Rate ASTM D 3985 cc/m²/24h
≤ 0.10 ≤ 0.10 ≤ 0.10
STORAGE & HANDLING

NAHAROPP™ does not require special storage conditions. it is recommended to storage below 30°C in order to avoid any deterioration of the film surface properties. it is advisable to use the material on FIFO basis. The film should be kept at operating environment for 24 hours before processing. material should be use before 3 months from dispatch

FOOD CONTACT

NAHAROPP™ Follow with EC and FDA regulations. MSDS are available on customer request.

DISCLAIMER

The values given in this technical datasheet are typical performance data and are believed to be accurate .These are given in good faith but it is for the customer to satisfy of the suitability for its own particular purpose. NAHAR POLY FILMS LTD. Suggests to the customer to confirm these values and product compatibility prior to their use and the company offers neither guarantee nor accept any responsibility for the fitness of the product for any other use.

NTM: NAHAR TEST METHOD, MD : MACHINE DIRECTION ,TD : TRANSVERSE DIRECTION

Updated on : 31 March 2023